Назва: | Fire-Resistant Coatings, Obtained by Layer-by-Layer Assembly, in the System of Silicic Acid Gel – Diammonium Hydrogen Phosphate – Urea |
Автори: | Курепін, Вячеслав Миколайович Kurepin, Vyacheslav Skorodumova, Olga Sharshanov, Andrey Chebotaryova, Olena Sotiriadis, Konstantinos |
Ключові слова: | cotton-containing textile materials fire resistance fire-resistant coatings layer-by-layer assembly liquid glass SiO2 sols sol-gel method |
Дата публікації: | 2023 |
Видавництво: | Mykolayiv national agrarian university National University of Civil Defence of Ukraine Institute of Theoretical and Applied Mechanics of the Czech Academy of Sciences |
Бібліографічний опис: | Skorodumova, O., Sharshanov, A., Chebotaryova, O., Kurepin, V., & Sotiriadis, K. (2023). Fire-Resistant Coatings, Obtained by Layer-by-Layer Assembly, in the System of Silicic Acid Gel – Diammonium Hydrogen Phosphate – Urea. Key Engineering Materials, 954, 157–165. https://doi.org/10.4028/p-s5rvla |
Короткий огляд (реферат): | The paper discusses the influence of flame retardant compositions obtained in the system of silicic acid sol (SiO2 sol) – flame retardants on the fire retardant properties of thin dense cotton fabrics and low density voluminous tapestry fabrics. The need to develop the optimal composition of a fire-retardant composition for a specific fabric, or to unify it for two main groups of fabric: thin and bulky low-density ones, is substantiated. Experimental coatings were obtained by applying SiO2 sol, which was obtained by the reaction between liquid glass and acetic acid, followed by application of flame retardant solutions (diammonium hydrogen phosphate (DAHP) and urea) by spraying or by the bath method. As a result of the optimization, using the central composite uniform rotatable plan of the second order, it was established that the main effect of the flame retardant is exerted by diammonium hydrogen phosphate (DAHP). The content or concentration of urea depends on the concentration of DAHP used: if diluted DAHP solutions (9–10 %) are used, trace amounts of urea (0–0.5 %) must be added. In the case of using a concentrated DAHP solution (18–20 %), the concentration of the urea solution should also be increased to 8–10 %. © 2023 Trans Tech Publications Ltd, Switzerland. |
Опис: | Повний текст статті доступний з сайту видання за посиланням: https://www.scientific.net/KEM.954.157 |
URI (Уніфікований ідентифікатор ресурсу): | https://dspace.mnau.edu.ua/jspui/handle/123456789/15144 |
Розташовується у зібраннях: | Публікації науково-педагогічних працівників МНАУ у БД Scopus Статті (Інженерно-енергетичний факультет) |
Файли цього матеріалу:
Файл | Опис | Розмір | Формат | |
---|---|---|---|---|
Fire-Resistant Coatings-2023.pdf | 2,51 MB | Adobe PDF | Переглянути/Відкрити |
Усі матеріали в архіві електронних ресурсів захищені авторським правом, всі права збережені.